malmi mahu suurenemine tingituna karbiidide, peamiselt tsementiidi (Fe3C) lagunemisest (grafitiseerumisest) või oksüdeerumisest t°-l üle 480 °C
a permanent increase in the dimensions of cast iron resulting from repeated or prolonged heating temperatures above 480 oC due to either to graphitizing of carbides or oxidation