Domain strength of materialswelding - design - equipment - testingtesting methods
  • temperatuur, mille juures metalli murdepinna makrostruktuur hakkab muutuma valdavalt plastsest valdavalt (vrd plastse murde siirdetemperatuur, hapra murde siirdetemperatuur)
    Good to know
    • Plastne-habras siirdetemperatuur, mille juures metalli murdepinna makrostruktuurile on iseloomulik 50% plastset ja 50% habrast murdu.
  • a specific temperature at which the fracture appearance of a metal changes from being predominently ductile to predominantly brittle (compare: fracture transition plastic temperature, nil-ductility transition temperature)
    Good to know
    • The temperature at which the fracture is 50% ductile and 50% brittle.
fracture appearance transition temperature preferred
FATT

Word forms not available

Etymology not available

Related words not available

Search the same word

in the EU's IATE term base

Web examples

Online Language Learning Tool SkELL allows users to search for phrases in sentences, collocates and similar words. These examples have been automatically selected and may contain errors.