shrinkage rate of timber
shrinkage rate varies considerably from species to species, but as a rough rule-of-thumb, wood undergoes about 8 % tangential shrinkage, 4 % radial shrinkage, and 0,1 % longitudinal shrinkage from the green to ovendry condition, kahanemistegur, mis on puu kuivamisel liikide lõikes märkimisväärselt erinev